Ink and Chemicals / Re: Yoga Mats?
« Last post by Admiral on Today at 03:24:16 PM »I found this quickly:
"Just called Nazdar and talked to Dan Miller. He said the DA series with DA 176 catalyst is the best for EVA foam. It takes about 24 hours to cross link and should be printed through a 110"
Source:Reddit
Sounds like what you were about to do.
"Just called Nazdar and talked to Dan Miller. He said the DA series with DA 176 catalyst is the best for EVA foam. It takes about 24 hours to cross link and should be printed through a 110"
Source:Reddit
Sounds like what you were about to do.