So we had Sonny(printficient) come in yesterday and he really helped.
We decided there are about 2-3 things that need attention:
1. chemicals. The dehaze is either missing stuff or leaving a residue on the mesh. We are adding a stronger degrease in for the time being to see if that helps.
2. flash. We lowered the heat and upped the time. We are flashing in 1.5 seconds, no way we are printing that fast, so we are slowing the flash time to our fastest production speed
3. angle. We went to 2-3 degrees instead of 5.
Testing was great, but we of course won't know until we get into production and right now we are caught up so our press op has the day off. It all looks promising. I really don't want to get into mixing a special white, but i'm not opposed to it. That may be the next step.