TSB

screen printing => Waterbase and Discharge => Topic started by: noortrd on November 04, 2013, 01:47:55 PM

Title: discharge washing
Post by: noortrd on November 04, 2013, 01:47:55 PM
Anybody face problem in discharge washing .
ourenduser face problem in pc fabric . they
need good white on pc fabric so they apply 2
or three stroke of magna super white . But
washing failed . They use discharge bcs foil
not attract to discharge. There also a foil print.
Any help . What about cci and rutland.? Any help.

Title: Re: discharge washing
Post by: dirkdiggler on November 04, 2013, 02:13:01 PM
Magna super white WILL NOT FAIL, if you following directions.  Sounds like its not cured.  I use it with 0 problems.
Title: Re: discharge washing
Post by: noortrd on November 05, 2013, 09:07:20 AM
yes its good for cotton but pc the washing fail. Is ther any help ?.
Title: Re: discharge washing
Post by: jvanick on November 05, 2013, 09:33:41 AM
I assume you mean P/C as polycotton blend?

Discharge doesn't work well on some blends, heck, sometimes it doesn't even work well in the same run of shirts if the shirts are from different 'lots'.