Author Topic: ? for those using Low Cure Temp additive  (Read 1770 times)

Offline ZooCity

  • Gonzo Member
  • ******
  • Posts: 4914
? for those using Low Cure Temp additive
« on: November 06, 2013, 04:57:09 PM »
Is it OK for use with Liquid Silver or a shimmer?  We have a run on polys where client would like a metallic but I want that cure temp dropped.

Thanks in advance.


Online Frog

  • Administrator
  • Ludicrous Speed Member
  • *****
  • Posts: 13952
  • Docendo discimus
Re: ? for those using Low Cure Temp additive
« Reply #1 on: November 06, 2013, 06:03:31 PM »
Can't say from experience, but the base is a fully curable complete base so why not?
Of course, you still have to deal with the fact that the reflectivity(is that a word?) messes with you a bit.
That rug really tied the room together, did it not?

Offline ZooCity

  • Gonzo Member
  • ******
  • Posts: 4914
Re: ? for those using Low Cure Temp additive
« Reply #2 on: November 06, 2013, 07:00:29 PM »
Indeed, that's why I'm looking to drop the cure temp of the carrier base.  I think it's likely the only option, unless someone is making a low cure metallic but I doubt it.